Search
Now showing items 1-4 of 4
Accelerated weathering effects on poly(3-hydroxybutyrate-co-3-hydroxyvalerate) (PHBV) and PHBV/TiO2 nanocomposites
(
MDPI AG
, 2020 , Article)
The effect of accelerated weathering on poly(3-hydroxybutyrate-co-3-hydroxyvalerate) (PHBV) and PHBV-based nanocomposites with rutile titanium (IV) dioxide (PHBV/TiO2) was investigated. The accelerated weathering test ...
Effects of rutile-TiO2 nanoparticles on accelerated weathering degradation of poly(Lactic Acid)
(
MDPI AG
, 2020 , Article)
The effect of accelerated weathering on poly(lactic acid) (PLA) and a PLA nanocomposite with rutile titanium (IV) dioxide (rutile-TiO2) was investigated. The accelerated weathering test applied consecutive steps of ultraviolet ...
Effect of plasma treatment on accelerated pla degradation
(
BME-PT and GTE
, 2021 , Article)
Poly(lactic acid) (PLA) has been found to be important in various applications, such as in the medical, pharma-ceutical, and packaging industries. However, the long-term associated degradation process of PLA is a limiting ...
Adhesive properties of polyester treated by cold plasma in oxygen and nitrogen atmospheres
(2013 , Article)
Polyester foil was treated by the surface diffuse barrier discharge (SDBD) plasma at atmospheric pressure in oxygen and/or in nitrogen containing a small amount of oxygen to improve its surface and adhesive properties. ...