High temperature thermal stability of innovative nanostructured thin coatings for advanced tooling
( Trans Tech Publications Ltd , 2014 , Article)Tools for machining are made of hard steels and cemented carbide (WC-Co). For specialized applications, such as aluminium machining, diamond or polycrystalline cubic boron nitride are also used. The main problem with steel, ...