Search
Now showing items 1-10 of 17
Eco-friendly foam biocomposites based on cellulose extracted from date palm leaves and low-density polyethylene
(
Web Portal IOP
, 2020 , Article)
The design of composite materials using environmentally compatible materials and adopting sustainable preparation techniques is very necessary for a better environment. The present study is a step towards developing an ...
Accelerated weathering effects on poly(3-hydroxybutyrate-co-3-hydroxyvalerate) (PHBV) and PHBV/TiO2 nanocomposites
(
MDPI AG
, 2020 , Article)
The effect of accelerated weathering on poly(3-hydroxybutyrate-co-3-hydroxyvalerate) (PHBV) and PHBV-based nanocomposites with rutile titanium (IV) dioxide (PHBV/TiO2) was investigated. The accelerated weathering test ...
Effects of rutile-TiO2 nanoparticles on accelerated weathering degradation of poly(Lactic Acid)
(
MDPI AG
, 2020 , Article)
The effect of accelerated weathering on poly(lactic acid) (PLA) and a PLA nanocomposite with rutile titanium (IV) dioxide (rutile-TiO2) was investigated. The accelerated weathering test applied consecutive steps of ultraviolet ...
Influence of accelerated weathering on the physical and structural properties of poly(Lactic-acid)/ poly(3-hydroxybutyrate-co-3-hydroxyvalerate) (pla/phbv) blends
(
BME-PT and GTE
, 2021 , Article)
The paper aims to study the poly(lactic acid) (PLA) and poly(3-hydroxybutyrate-co-3-hydroxyvalerate) (PHBV) blend properties after their degradation under 2000 h of accelerated weathering conditions following the ASTM D4329 ...
Effect of plasma treatment on accelerated pla degradation
(
BME-PT and GTE
, 2021 , Article)
Poly(lactic acid) (PLA) has been found to be important in various applications, such as in the medical, pharma-ceutical, and packaging industries. However, the long-term associated degradation process of PLA is a limiting ...
Effect of poly(ε-caprolactone) and titanium (IV) dioxide content on the UV and hydrolytic degradation of poly(lactic acid)/poly(ε-caprolactone) blends
(
John Wiley and Sons Inc
, 2021 , Article)
The effect of accelerated weathering degradation on the properties of poly(lactic acid) (PLA)/poly(ε-caprolactone) (PCL) blends and PLA/PCL/titanium (IV) dioxide (TiO2) nanocomposites are presented in this paper. The results ...
Effect of plasma treatment on accelerated pla degradation
(
BME-PT and GTE
, 2021 , Article)
Poly(lactic acid) (PLA) has been found to be important in various applications, such as in the medical, pharma-ceutical, and packaging industries. However, the long-term associated degradation process of PLA is a limiting ...
Morphology analysis
(
Elsevier
, 2020 , Book chapter)
This chapter is dedicated to the surface morphology and topography analyses of various types of polymers in terms of their structural conformations and resulting material structures. The morphology of polymers includes ...
Sulfobetaine-based polydisulfides with tunable upper critical solution temperature (UCST) in water alcohols mixture, depolymerization kinetics and surface wettability
(
Academic Press Inc.
, 2021 , Article)
Hypothesis: Synthesis of a new family of polymers having a polydisulfide structure can be conducted from sulfobetaine-based derivative of natural (R)-lipoic acid. A polydisulfide backbone of polymer can be depolymerized ...
Probing the fibrillation of lysozyme by nanoscale-infrared spectroscopy
(
Taylor and Francis Ltd.
, 2021 , Article)
Amyloid fibrillation is the root cause of several neuro as well as non-neurological disorders. Understanding the molecular basis of amyloid aggregate formation is crucial for deciphering various neurodegenerative diseases. ...