Insights into the degradation mechanism of PET and PP under marine conditions using FTIR
Author | Sarra N., Dimassi |
Author | Hahladakis, John N. |
Author | Yahia, Mohamed Najib Daly |
Author | Ahmad, Mohammad I. |
Author | Sayadi, Sami |
Author | Al-Ghouti, Mohammad A. |
Available date | 2023-01-17T04:43:46Z |
Publication Date | 2023-01-14 |
Publication Name | Journal of Hazardous Materials |
Identifier | http://dx.doi.org/10.1016/j.jhazmat.2023.130796 |
Citation | Sarra N. Dimassi, John N. Hahladakis, Mohamed Najib Daly Yahia, Mohammad I. Ahmad, Sami Sayadi and Mohammad A. Al-Ghouti, Insights into the degradation mechanism of PET and PP under marine conditions using FTIR, Journal of Hazardous Materials, (2022) doi:https://doi.org/10.1016/j.jhazmat.2023.130796 |
ISSN | 03043894 |
Abstract | Plastics possess diverse functional properties that have made them extremely desirable. However, due to poor waste management practices, large quantities eventually end up in the oceans where their degradation begins. Hence, it is imperative to understand and further investigate the dynamics of this process. Currently, most relevant studies have been carried out under benign and/or controlled weather conditions. This study investigates the natural degradation of polypropylene (PP) and polyethylene terephthalate (PET) in more extreme environments. Simulated and real marine conditions, both in the laboratory (indoors) and outdoors were applied for a duration of 140 days and results were assessed using Fourier-transform infrared spectroscopy (FTIR) and scanning electron microscopy (SEM) with energy dispersive X-ray analysis. SEM micrographs revealed variations in the morphologies of both plastic types. Degradation signs were shown in both plastic types, under all conditions. Findings indicated that microplastics (MPs) degraded faster than macroplastics, with PP MPs having higher weight loss (49%) than PET MPs (1%) when exposed to outdoor marine conditions. Additionally, the degradation rates of MPs-PP were higher than MPs-PET for outdoor and indoor treatments, with 1.07 ×10-6g/d and 4.41 ×10-7g/d, respectively. FTIR combined with PCA was efficient in determining the most degraded plastic types. |
Sponsor | This paper was supported by Qatar University Internal Grant (No. QUCG-CAS-21/22-3). The findings achieved herein are solely the responsibility of the authors. The SEM-EDX, DSC, and FTIR analyses were accomplished in the Central Laboratories unit, Qatar University. |
Language | en |
Publisher | Elsevier |
Subject | Plastic waste degradation fragmentation marine litter FTIR |
Type | Article |
Volume Number | 447 |
ESSN | 1873-3336 |
Check access options
Files in this item
This item appears in the following Collection(s)
-
Biological & Environmental Sciences [920 items ]
-
Center for Sustainable Development Research [317 items ]
-
Central Laboratories Unit Research [101 items ]
-
Chemistry & Earth Sciences [587 items ]