المؤلفRamesh, A.
المؤلفLaycock, N.
المؤلفShenai, P.
المؤلفBarnes, A.
المؤلفVan Santen, H.
المؤلفThyagarajan, A.
المؤلفAbdullah, A. M.
المؤلفRyan, M. P.
تاريخ الإتاحة2025-07-03T05:56:03Z
تاريخ النشر2022-07-01
اسم المنشورCorrosion
المعرّفhttp://dx.doi.org/10.5006/4085
الاقتباسA. Ramesh, N. Laycock, P. Shenai, A. Barnes, H. Van Santen, A. Thyagarajan, A. M. Abdullah, M.P. Ryan; Critical Deposit Loading Thresholds for Under Deposit Corrosion in Steam Generators. CORROSION 1 July 2022; 78 (7): 584–598. https://doi.org/10.5006/4085
الرقم المعياري الدولي للكتاب00109312
معرّف المصادر الموحدhttps://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=85139044006&origin=inward
معرّف المصادر الموحدhttp://hdl.handle.net/10576/65940
الملخصSignificant industrial facilities typically operate a steam system with multiple steam generators (or boilers) that are potentially vulnerable to under deposit corrosion (UDC). This mechanism begins with the deposition of a porous layer of magnetite particles on the waterside heat transfer surfaces. Beneath this layer, wick-boiling causes the concentration of contaminants (such as chlorides) until the concentration exceeds some critical threshold that results in rapid corrosion. Industry practice to mitigate this risk includes monitoring the extent of deposition and then chemically cleaning the equipment before the deposits reach the critical level. One significant factor in this mechanism is the heat flux, which drives both the magnetite deposition and the wick-boiling processes. This paper investigates the relationship between heat flux and the critical deposit thickness for the initiation of chloride-driven UDC. Ex-service samples from industrial steam generators have been examined, an electrochemical method has been developed for in situ measurement of the deposit loading, and a wick-boiling model has been used to estimate the local conditions beneath the porous deposits during the progress of UDC. For 1.0 Cr 0.5 Mo steel coils from a steam generator operating at approximately 75 bar(a) under an all volatile treatment regime, the threshold for the onset of rapid UDC was determined to be at a heat flux of 350 kW/m<sup>2</sup>, deposit loading of approximately 50 mg/cm<sup>2</sup>, and deposit thickness of approximately 95 μm, corresponding to a local chloride concentration beneath the deposits of approximately 80 ppm and a local at-temperature pH below ∼2.7.
راعي المشروعThe project is made possible by the National Priorities Research Program-Standard (NPRP-S) Tenth Cycle Grant No. NPRP12S-0228-190182 from the Qatar National Research Fund (a member of Qatar Foundation). We would also like to acknowledge Dr. Ram Ratnakar (Shell Technology Center, Houston) for his contributions to the development of the wick-boiling model for this paper.
اللغةen
الناشرNACE International
الموضوعboiler
deposit
pitting
steam
under deposit corrosion
العنوانCritical Deposit Loading Thresholds for Under Deposit Corrosion in Steam Generators
النوعArticle
الصفحات584-598
رقم العدد7
رقم المجلد78