Rapid microwave assisted sol-gel synthesis of CeO2 and CexSm1-xO2 nanoparticle catalysts for CO oxidation
View/ Open
Publisher version (Check access options)
Check access options
Date
2016-11-30Author
Polychronopoulou, K.Zedan, Abdallah F.
Katsiotis, M.S.
Baker, M.A.
AlKhoori, A.A.
AlQaradawi, Siham Y.
Hinder, S.J.
AlHassan, Saeed
...show more authors ...show less authors
Metadata
Show full item recordAbstract
CeO2 and CexSm1-xO2 nanoparticle mixed oxides have been synthesized by microwave assisted sol-gel (MW sol-gel) and conventional sol-gel synthesis carried out at 60°C (typical sol-gel) and 100°C (approaching the MW temperature). Different characterization techniques, namely, XRD, BET, Raman, SEM, FTIR, TEM, XPS, H2-TPR, CO2-TPD, and XPS have been employed to understand the process-structure-properties relationship of the catalysts. The CO oxidation performance has been determined both in the absence and in the presence of H2 in the feed gas stream. Microwave heating yields a more thermally stable precursor material, which preserves 75% of its mass up to 600°C, attributable to the different chemical nature of the precursor, compared to the typical sol-gel material with the same composition. Varying the synthesis method has no profound effect on the surface area of the materials, which is in the range 4–35m2/g. Conventional sol-gel synthesis performed at 60 and 100°C yields CeO2 particles with a crystallite size of 29nm and 24nm compared to 21–27nm for MW sol-gel synthesis (at different power values). The MW sol-gel CexSm1-xO2 catalysts exhibit a smaller crystallite size (12–18nm). The pure ceria nanoparticles were shown to have a stoichiometry of approximately CeO1.95. The presence of Ce3+ and Sm3+ in the mixed oxide particles facilitates the presence of oxygen vacant sites, confirmed by Raman. Oxygen mobile species have been traced using H2-TPR studies and a compressive lattice strain in the 0.45–1.9% range of the cubic CexSm1-xO2 lattice were found to be strongly correlated with the CO oxidation performance in the presence and absence of H2 in the oxidation feed stream. MW sol-gel synthesis led to more active CeO2 and Ce0.5Sm0.5O2 catalysts, demonstrated by T50 (temperature where 50% CO conversion is achieved), being reduced by 131°C and 47°C, respectively, compared to typical sol-gel catalysts. Conventional synthesis performed at 100°C leads to a CeO2 catalyst of initially higher activity at a certain temperature window (220–420°C), though with a slower increase of XCO as a function of temperature compared to the MW synthesized catalyst. MW sol-gel synthesized Ce0.8Sm0.2O2 exhibited a high performance (∼90%) for CO oxidation over a period of more than 20h in stream. In addition the effect of reaction temperature and contact time (W/F) on the activity of the CeO2-based materials for CO oxidation kinetics were investigated. The activation energy of the reaction was found to be in the range 36–43kJ/mole depending on the catalyst composition.
Collections
- Chemistry & Earth Sciences [587 items ]