الملخصThis paper reports on the thermal degradation behaviour and kinetics of halloysite nanotubes containing microfibrillated poly(ε-caprolactone) (PCL)/poly(lactic acid) (PLA) blends. It was found that the nanotubes probably catalyzed the PLA degradation, and that the free radicals formed during the PLA degradation initiated PCL degradation at lower temperatures, maybe in combination with halloysite nanotubes (HNT) catalysis. Drawing to form microfibrillated nanocomposites had little influence on the degradation behaviour of these materials, but pre-mixing of the HNT with PLA or PCL prior to melt-mixing and extrusion-drawing of the blends did influence the degradation behaviour, but in different ways. No evidence could be found that the presence and amount of HNT, or the mode of preparation, had an influence on the degradation mechanism, as evidenced through a Fourier-transform infrared (FTIR) analysis of the degradation products.
راعي المشروعThis work was supported by Czech Science Foundation (Grant No 13-15255S), while the Center for Advanced Materials at Qatar University provided the infrastructure for conducting the experimental work.
اللغةen
الناشرElsevier Ltd
الموضوعHalloysite nanotubes
Nanocomposites
Poly(lactic acid)
Poly(?-caprolactone)
Thermal degradation
العنوانEffect of halloysite nanotubes on the thermal degradation behaviour of poly(ε-caprolactone)/poly(lactic acid) microfibrillar composites
النوعArticle
الصفحات166-172