Effect of halloysite nanotubes on the thermal degradation behaviour of poly(ε-caprolactone)/poly(lactic acid) microfibrillar composites
Author | Luyt, Adriaan S. |
Author | Kelnar, Ivan |
Available date | 2021-01-27T11:06:56Z |
Publication Date | 2017 |
Publication Name | Polymer Testing |
Resource | Scopus |
ISSN | 1429418 |
Abstract | This paper reports on the thermal degradation behaviour and kinetics of halloysite nanotubes containing microfibrillated poly(ε-caprolactone) (PCL)/poly(lactic acid) (PLA) blends. It was found that the nanotubes probably catalyzed the PLA degradation, and that the free radicals formed during the PLA degradation initiated PCL degradation at lower temperatures, maybe in combination with halloysite nanotubes (HNT) catalysis. Drawing to form microfibrillated nanocomposites had little influence on the degradation behaviour of these materials, but pre-mixing of the HNT with PLA or PCL prior to melt-mixing and extrusion-drawing of the blends did influence the degradation behaviour, but in different ways. No evidence could be found that the presence and amount of HNT, or the mode of preparation, had an influence on the degradation mechanism, as evidenced through a Fourier-transform infrared (FTIR) analysis of the degradation products. |
Sponsor | This work was supported by Czech Science Foundation (Grant No 13-15255S), while the Center for Advanced Materials at Qatar University provided the infrastructure for conducting the experimental work. |
Language | en |
Publisher | Elsevier Ltd |
Subject | Halloysite nanotubes Nanocomposites Poly(lactic acid) Poly(?-caprolactone) Thermal degradation |
Type | Article |
Pagination | 166-172 |
Volume Number | 60 |
Check access options
Files in this item
Files | Size | Format | View |
---|---|---|---|
There are no files associated with this item. |
This item appears in the following Collection(s)
-
Center for Advanced Materials Research [1378 items ]