Effect of halloysite nano tubes on the thermal degradation behaviour of PCL/PLA microfibrillar composites
المؤلف | Luyt, A.S. |
المؤلف | Kelnar, I. |
تاريخ الإتاحة | 2018-07-11T10:02:53Z |
تاريخ النشر | 2017 |
اسم المنشور | Polymer Testing |
المعرّف | http://dx.doi.org/10.1016/j.polymertesting.2017.03.027 |
الاقتباس | L. Adriaan S. ,K. Ivan. Effect of halloysite nanotubes on the thermal degradation behaviour of poly(ε-caprolactone)/poly(lactic acid) microfibrillar composites.(2017). Polymer Testing, Volume 60, P.p. 166-172 |
الرقم المعياري الدولي للكتاب | 0142-9418 |
الملخص | This paper reports on the thermal degradation behaviour and kinetics of halloysite nanotubes containing microfibrillated poly(ε-caprolactone) (PCL)/poly(lactic acid) (PLA) blends. It was found that the nanotubes probably catalyzed the PLA degradation, and that the free radicals formed during the PLA degradation initiated PCL degradation at lower temperatures, maybe in combination with halloysite nanotubes (HNT) catalysis. Drawing to form microfibrillated nanocomposites had little influence on the degradation behaviour of these materials, but pre-mixing of the HNT with PLA or PCL prior to melt-mixing and extrusion-drawing of the blends did influence the degradation behaviour, but in different ways. No evidence could be found that the presence and amount of HNT, or the mode of preparation, had an influence on the degradation mechanism, as evidenced through a Fourier-transform infrared (FTIR) analysis of the degradation products. |
اللغة | en |
الناشر | Elsevier |
الموضوع | Poly(lactic acid); Poly(ε-caprolactone); Halloysite nanotubes; Nanocomposites; Thermal degradation Poly(lactic acid) Poly(ε-caprolactone) Halloysite nanotubes Nanocomposites Thermal degradation |
النوع | Article |
الصفحات | 166-172 |
رقم المجلد | 60 |
ESSN | 1873-2348 |
تحقق من خيارات الوصول
الملفات في هذه التسجيلة
الملفات | الحجم | الصيغة | العرض |
---|---|---|---|
لا توجد ملفات لها صلة بهذه التسجيلة. |
هذه التسجيلة تظهر في المجموعات التالية
-
الأبحاث [1449 items ]